Serious question, does normalizing steel after forging beat just letting it air cool?
Had a batch of 1084 blades come out with warped edges last month, so I ran a normalizing cycle (heat to 1600F, air cool, repeat twice) before the quench and they came out dead straight. Half the old timers at my shop say normalizing is extra work for nothing on simple carbon steel, but my results say otherwise. What do you all do on your blades?