The old finisher at the shop in Reno got me to switch to a wood float on my first pass
I used to go straight to the magnesium float on every slab, figured wood was just extra work. Then Ray, who has been finishing for 31 years, watched me pull a 12x20 patio and told me the mag float was sealing the surface too fast in that dry Nevada heat. Tried the wood float first on the next pour and my edges came out way cleaner, no tearing when I went back over them. Anyone else switch their first pass based on the weather instead of habit?
Man, that bit about Ray watching you pull a whole patio before saying anything hits home. Guys with that many years usually let you mess up first, then drop the fix like it's nothing. Dry heat really does change everything, the mud goes off way faster than people expect and the mag float just locks it in. Good on you for actually trying it instead of sticking with the habit.