Warning: my 12 yard pour in Tucson started setting up on me in 85 degree heat and I had to think fast
Was finishing a driveway slab out in Tucson last Thursday and the mix started going off way faster than I planned for. I had two guys on floats and the edge was already stiff at about 40 minutes, which is not what you want when you still have a whole back corner to work. I told my finisher to stop floating and we hit the whole thing with a retarder spray, then covered it with plastic to buy us some time. We ended up working it in two sections instead of one pass, which meant a cold joint I'm not happy about but the surface came out clean. Waited until it was cool enough to trowel and went over the seam with a hand float to blend it as best I could. Next time I'm ordering the mix with a slower set time no matter what the batch plant says about the weather. Anyone got a go-to slump or admixture setup for hot weather pours that keeps the finish workable?
Funny how the heat always shows you what a mix is really made of, kind of like how people act different when things get stressful. Glad the surface came out clean at least.